Check your z-offset, it looks like nozzle may be scraping the bed. With very minimal bed leveling issues this will cause big problems. Try moving the nozzle a bit further away.
3DPrinting
3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.
The r/functionalprint community is now located at: or !functionalprint@fedia.io
There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml
Rules
-
No bigotry - including racism, sexism, ableism, homophobia, transphobia, or xenophobia. Code of Conduct.
-
Be respectful, especially when disagreeing. Everyone should feel welcome here.
-
No porn (NSFW prints are acceptable but must be marked NSFW)
-
No Ads / Spamming / Guerrilla Marketing
-
Do not create links to reddit
-
If you see an issue please flag it
-
No guns
-
No injury gore posts
If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![]()
Moderation policy: Light, mostly invisible
Hard to tell, most of it looks fairly good except a few spots here and there.
That could be grease on the print bed, maybe time to give it a wash? When PETG goes wrong for me, it's this 90% of the time.
I use hot water and a little detergent with a lot of rinsing. Use gloves because even clean hands leave oils behind.
With PETG it's hard to get the first layer right but if it's good the rest of the print generally goes fine.
Molten PETG is very sticky and if you get a bit stuck to the nozzle it can build up, get worse and suddenly take out a bunch of nearby lines leading to gaps in the layer like this.
To counter this PETG first layer should be:
- Printed very slow e.g. 20mm/s
- At a higher Z offset than PLA, the plastic should flow out the nozzle and fall onto the bed rather than be squished flat.
- High bed temperature 80C / 176F
- Zero or very low fan speed for the first couple of layers
If you can see marks left by the nozzle it's too low. The lines should have a rounded look.
It could also be wet filament, does it make popping sounds when printing?
To start, your z offset is too high, your nozzle isnt close enough to the bed. Your lines should not have gaps like that, gapping in your lines means the nozzle isnt close enough to the bed to "squish" the plastic outwards and join with the adjacent line. Im gonna go out on a limb and guess this print peels off the ned very easily, and as you pull it up and off it sprt of "splinters" a bit, parts of it "fall apart" right?
If you get your z offset right, the print should come off as 1 solid piece without gapping.
Quick question:
If you run it the same time, are the failings in the exact same spots, or different spots?
Exact same spots
Bed issues, or physical issues perhaps with the wire harness to your heater catching or stretching, causing hiccups. Watch as it prints the problem areas for physical issues like it bumping stuff, or scraping on things, the wire harness, etc.
Almost same spots but not exact same
Flow issues, lower print speed 20%, see if it improves a bunch. Your nozzle is backing up and then surging causing inconsistent pressure on long runs.
Different spots
Check your z offset and watch your spool as it spins, if your spool is catching everytime it turns, it'll inflict random jerks on your nozzle. Also check tightness on your movement system, it might be loose and getting perked a bunch by pulling on the spool as it works through the filament.
Could be multiple things. Dry your filament, in an oven or special dry box if you own one. Clean your bed with warm water (no soap or alcohol/acetone)
Use a glue stick for better adhesion.
Also, if you printer support it, you can generate a level matrix to see if it is leveled.
Why no soap? I clean with dish soap to remove oils, works great.
It also looks very thin, check your Z offset.
Increase bed temp 5 degrees, lower z offset by a few hundreths, and throw a trash bag over the printer to create a makeshift enclosure.
The z offset will likely have the biggest impact. Textured beds need to have their offset lowered to squish the plastic into the texture a bit more. The auto offset tends to detect the top of the texture as if it were a smooth plate. Your print is also showing some distinct separation lines on the first layer. For my Ender 3, I usually started by lowering my z offset by -0.07 mm.
Bed temp increase will help adhesion. Trash bag will help with curling, which PETG loves to do.
I don't think bed leveling issues would look like that; it could be dirty bed of course, but also what temperature bed & hotend are you using?
Looks wet to me.
How long did you dry it for? 3 hours? I generally give it six (or more).
People are obsessed with babying their filaments; I’ve never met a problem that wasn’t solved by changing nozzle temp.
Lucky person that doesn't live in humidity. I been zip lock bagging my filament after every use. If I leave PLA out for more than a day it's the death of printing.