this post was submitted on 15 Jul 2023
7 points (100.0% liked)

3DPrinting

19254 readers
107 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![]()

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 

I'm changing the PTFE in my heatbreak, I didn't realize these seem to be consumables. It started causing blockage.

A guy sent me a piece of PTFE from his Prusa MK3S+ that I could try as i was having trouble finding any PTFE quickly.

I realized I couldn't just cut a piece and put it in, that caused a lot of filament leakage and underextrusion. The end of the PTFE toward the nozzle was a bit jagged and I believe that's where the leakage happened. Now I'm wondering how the heatbreak and nozzle normally interface inside the heatblock, should they be touching? Should the PTFE protrude a bit from the heatbreak so there's a bit of pressure against the nozzle when I screw it in?

you are viewing a single comment's thread
view the rest of the comments
[–] MrSlicer@lemmy.world 3 points 2 years ago

When you order bowden tube it comes with a cutter. Make sure your fittings are tight.

But also heat up the hotend remove the nozzle and tube. Then push in through a piece of old bowden tube. This ensures there is no remaking plastic in the throat. Now reassemble. the old ptfe tu