this post was submitted on 26 Jan 2026
49 points (96.2% liked)

3DPrinting

21110 readers
68 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![]()

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 

Hi! Looking for some advice here from friendly local experts.

I've printed this with Elegoo Neptune 3 Pro, 0.4 nozzle, Elegoo PETG filament, no enclosure. Using PrusaSlicer.

This print is basically all walls - the hex grid is thin. It's 2mm thick and each segment is 1.5mm wide. I set 3 layers for walls in slicer. It was printed vertically, just as seen on picture.

The solid part of the print (back wall) came out just fine, but the hex grid part came... dirty. On the picture, there are a few hex segments that just broke off during the print at the base of vertical segments. And the rest of them have small loops of filament that stick outside of the intended surface, to the sides.

My suspicion is the print temperature is too low. I'm printing at 230, which is the low end of 230-260 range of the filament. But in my previous tests I noticed stringing that starts around 240, so I did a few other prints that were just fine at 230, and I made it my default temp for this spool.

Or is it just too fine detail for my printer with PETG? Or something else that I am missing?

you are viewing a single comment's thread
view the rest of the comments
[–] kahjtheundedicated@lemmy.world 17 points 2 days ago (3 children)

Looks like a filament moisture issue to me. PETG can get real weird unless it’s really dry. Temp is also a little low, but drying the filament will also fix the stringing issues you were seeing at 240

[–] pound_heap@lemmy.dbzer0.com 4 points 2 days ago (2 children)

Thanks! I think I unpacked this filament about a month ago, and it was on open air for about two weeks, in 40-50% humidity. then I put it into a dry box with a box of silica gel, and it stays there at about 20% humidity. Until I take it out for a print. Is silica gel good enough for drying? I don't have the drying machine.

[–] fufu@feddit.org 1 points 16 hours ago

there is no issues with humidity

[–] kahjtheundedicated@lemmy.world 3 points 2 days ago (1 children)

Silica gel has worked pretty well for me to keep a spool dry for a couple months, but I’ve never tried to dry a “wet” spool with it, so no idea. I’ve dried petg spools in the oven before, and it worked out. Can’t remember what temperature, but I’m sure that’s floating around on the internet somewhere.

Also the silica gel only keeps stuff dry if it’s dry itself. You can also heat that in the oven or a microwave to do that.

So yeah I’ve found petg (or at least the cheap stuff I’ve bought) to be kind of a pain. But if you’re almost neurotic about keeping it dry, you can get some super nice results. I only use it if I really want something to be clear

[–] pound_heap@lemmy.dbzer0.com 1 points 2 days ago (3 children)

In the oven??? But wouldn't it just melt? I have a gas oven, I don't think it can go too low. But I will look it up. Maybe microwave is a way to go. Thanks for the tip.

[–] Scubus@sh.itjust.works 2 points 1 day ago

A lot of people use food dehydrators. You can even get a spool holder that feeds the filament to your printer and dries it at the same time.

[–] hperrin@lemmy.ca 3 points 1 day ago* (last edited 1 day ago)

Microwave will not work. Unless you’re incredibly careful/lucky, you’ll ruin your filament. You can use your printer’s heated bed to dry it. Look up how to do it online, but basically you lay it on the bed, put a box over it to enclose it, turn the bed to 55°, and let it dry like that for 10 hours. That’s for PLA though, so you may have to go hotter for PETG.

Silica gel works to keep it from getting wet, but it won’t work to dry it, since the filament wants to hold on to that water. The only way to get the water out is to use heat. (Or maybe a vacuum chamber, but heat is a lot easier.)

Yeah, my oven is electric. Internet says 65C, which is conveniently as low as my oven goes

[–] hperrin@lemmy.ca 5 points 2 days ago

Yes. This absolutely looks like a moisture issue. Drying the filament will almost definitely help.

[–] Midnattssol@feddit.nu 1 points 2 days ago

Yes, I second making sure the filament is well dried before printing. It usually fixes issues like this for me.